Thermal Properties | Metric | English | Comments |
---|---|---|---|
Specific Heat Capacity | 1.00 - 1.80 J/g-°C | 0.239 - 0.430 BTU/lb-°F | |
Goodfellow Polyvinyl Fluoride (PVF) Film A semi-crystalline, colorless, transparent-translucent fluoropolymer with excellent weathering resistance, good chemical resistance and low permeability to gases; it is very slow burning and has a v.. |