Thermal Properties Metric English Comments
Specific Heat Capacity 0.485 J/g-°C
0.116 BTU/lb-°F
ATI Allegheny Ludlum Altemp® HX Nickel-Based superalloy
Characteristics: outstanding resistance to oxidation at high temperatures, exceptional strength at elevated temperatures, good fabricability, good machinability in annealed condition, work hardening..