Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Specific Heat Capacity = 0.605 J/g-°C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Specific Heat Capacity 0.605 J/g-°C

@Temperature 800 °C
0.145 BTU/lb-°F

@Temperature 1470 °F
Haynes 242® alloy, cold reduced sheet, annealed, 20% cold work
Age-hardenable, high ductility in the aged condition, lower thermal expansion than most alloys, very good oxidation resistance up to 815°C, excellent low cycle fatigue properties, very good therm..
Specific Heat Capacity 0.605 J/g-°C

@Temperature 800 °C
0.145 BTU/lb-°F

@Temperature 1470 °F
Haynes 242® alloy
Age-hardenable, high ductility in the aged condition, lower thermal expansion than most alloys, very good oxidation resistance up to 815°C, excellent low cycle fatigue properties, very good therm..
Specific Heat Capacity 0.605 J/g-°C

@Temperature 800 °C
0.145 BTU/lb-°F

@Temperature 1470 °F
Haynes 242® alloy, after 1000 hours exposure at 650°C (1200°F)
Age-hardenable, high ductility in the aged condition, lower thermal expansion than most alloys, very good oxidation resistance up to 815°C, excellent low cycle fatigue properties, very good therm..
Specific Heat Capacity 0.605 J/g-°C

@Temperature 800 °C
0.145 BTU/lb-°F

@Temperature 1470 °F
Haynes 242® alloy, after 4000 hours exposure at 650°C (1200°F)
Age-hardenable, high ductility in the aged condition, lower thermal expansion than most alloys, very good oxidation resistance up to 815°C, excellent low cycle fatigue properties, very good therm..
Specific Heat Capacity 0.605 J/g-°C

@Temperature 800 °C
0.145 BTU/lb-°F

@Temperature 1470 °F
Haynes 242® alloy, after 8000 hours exposure at 650°C (1200°F)
Age-hardenable, high ductility in the aged condition, lower thermal expansion than most alloys, very good oxidation resistance up to 815°C, excellent low cycle fatigue properties, very good therm..
Specific Heat Capacity 0.605 J/g-°C

@Temperature 800 °C
0.145 BTU/lb-°F

@Temperature 1470 °F
Haynes 242® alloy, cold reduced sheet, annealed
Age-hardenable, high ductility in the aged condition, lower thermal expansion than most alloys, very good oxidation resistance up to 815°C, excellent low cycle fatigue properties, very good therm..
Specific Heat Capacity 0.605 J/g-°C

@Temperature 800 °C
0.145 BTU/lb-°F

@Temperature 1470 °F
Haynes 242® alloy, cold reduced sheet, annealed and 20% cold work
Age-hardenable, high ductility in the aged condition, lower thermal expansion than most alloys, very good oxidation resistance up to 815°C, excellent low cycle fatigue properties, very good therm..
Specific Heat Capacity 0.605 J/g-°C

@Temperature 800 °C
0.145 BTU/lb-°F

@Temperature 1470 °F
Haynes 242® alloy, cold reduced sheet, annealed and 40% cold work
Age-hardenable, high ductility in the aged condition, lower thermal expansion than most alloys, very good oxidation resistance up to 815°C, excellent low cycle fatigue properties, very good therm..
Specific Heat Capacity 0.605 J/g-°C

@Temperature 800 °C
0.145 BTU/lb-°F

@Temperature 1470 °F
Haynes 242® alloy, cold reduced sheet, annealed and aged
Age-hardenable, high ductility in the aged condition, lower thermal expansion than most alloys, very good oxidation resistance up to 815°C, excellent low cycle fatigue properties, very good therm..
Specific Heat Capacity 0.605 J/g-°C

@Temperature 800 °C
0.145 BTU/lb-°F

@Temperature 1470 °F
Haynes 242® alloy, cold reduced sheet, annealed, 40% cold work, aged
Age-hardenable, high ductility in the aged condition, lower thermal expansion than most alloys, very good oxidation resistance up to 815°C, excellent low cycle fatigue properties, very good therm..