Thermal Properties | Metric | English | Comments |
---|---|---|---|
Specific Heat Capacity | 0.760 J/g-°C | 0.182 BTU/lb-°F | |
Schott N-SF15 Glass Information Provided by SCHOTT North America, Inc. |
|||
Specific Heat Capacity | 0.760 J/g-°C | 0.182 BTU/lb-°F | |
Schott N-SF4 Glass Information Provided by SCHOTT North America, Inc. |
|||
Specific Heat Capacity | 0.760 J/g-°C | 0.182 BTU/lb-°F | |
Schott P-SK57 Glass Suitable for precision moldingInformation Provided by SCHOTT North America, Inc. |
|||
Specific Heat Capacity | 0.760 J/g-°C | 0.182 BTU/lb-°F | |
Schott N-KZFS4 Glass Information Provided by SCHOTT North America, Inc. |
|||
Specific Heat Capacity | 0.760 J/g-°C | 0.182 BTU/lb-°F | |
Schott N-KZFS8 Glass Information Provided by SCHOTT North America, Inc. |
|||
Specific Heat Capacity | 0.760 J/g-°C | 0.182 BTU/lb-°F | DSC |
Wolf Kunststoff ZEDEX® ZX-550 A5L Polymer Alloy Main Characteristics: Strong anti-adhesive; Low creep; Weather resistant; No water absorption; Good machinability; Strongly viscoelastic; Stress resistantApplications: Chemical Engineering; Laborato.. |
|||
Specific Heat Capacity | 0.760 J/g-°C | 0.182 BTU/lb-°F | E1461-01 |
Arlon Thermabond® 99720W015 0.015" Uncured Silicone Rubber with PTFE Coated Fiberglass Carrier Design/Construction:Liner: 0.001" FEP FilmSide 1: Uncured Silicone RubberCarrier: 0.003" PTFE coated FiberglassRecommended Primer: Dow Corning S2260This data represents typical values for the pr.. |