Thermal Properties | Metric | English | Comments |
---|---|---|---|
Specific Heat Capacity | 0.873 J/g-°C | 0.209 BTU/lb-°F | |
Constellium Certal® SPC Aluminum Certal® SPC has been optimized to provide excellent machinability, good shape stability and high strength properties throughout the plate thickness. Uniform strength is an important property in man.. |