Thermal Properties | Metric | English | Comments |
---|---|---|---|
Specific Heat Capacity | 0.962 - 1.05 J/g-°C | 0.230 - 0.251 BTU/lb-°F | |
Polikim EFALON® T-100 Virgin PTFE Applications: Gaskets, seals, O-rings, V-Rings, compression packings and similar sealing parts, Bushes, bearings and piston rings, Electrical insulators, Sliding supports, Conveyor belts, Coated tu.. |
|||
Specific Heat Capacity | 1.00 - 1.05 J/g-°C | 0.239 - 0.251 BTU/lb-°F | Average value: 1.01 J/g-°C Grade Count:6 |
Overview of materials for Polytetrafluoroethylene (PTFE), Molded This property data is a summary of similar materials in the MatWeb database for the category "Polytetrafluoroethylene (PTFE), Molded". Each property range of values reported is minimum and maximum v.. |