Polymer Property : Specific Heat Capacity = 1.172 J/g-°C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Specific Heat Capacity 1.172 J/g-°C

@Temperature 600 °C
0.2801 BTU/lb-°F

@Temperature 1110 °F
Zircar Refractory Composites RS-100 Refractory Sheet
ZIRCAR Refractory Sheet Type RS-100 is a ceramic fiber reinforced structural alumina composite material with useful properties to 1260°C (2300°F). It has exceptional flexural and compressive stren..
Specific Heat Capacity 1.172 J/g-°C

@Temperature 600 °C
0.2801 BTU/lb-°F

@Temperature 1110 °F
Zircar Refractory Composites RS-1200 Refractory Sheet
ZIRCAR Refractory Sheet Type RS-1200 is a high strength composite designed for use as thermo-mechanical and electrical insulation in applications with temperatures as high as 1300°C(2372°F). RS-12..