Thermal Properties | Metric | English | Comments |
---|---|---|---|
Specific Heat Capacity | 1.21 - 1.38 J/g-°C | 0.290 - 0.330 BTU/lb-°F | ASTM E1461-92 |
Park Electrochemical Nelco® N4000-2 Multifunctional Epoxy Laminate and Prepreg The Nelco® N4000-2 is the most established material of Nelco’s product line. This multifunctional epoxy laminate and prepreg system has a long history of use and one of the broadest operating and .. |
|||
Specific Heat Capacity | 1.21 - 1.38 J/g-°C | 0.290 - 0.330 BTU/lb-°F | ASTM E1461-92 |
Park Electrochemical Nelco® N4000-11 BC® Buried Capacitance™ Epoxy Laminate and Prepreg The Nelco® N4000-11 is a CAF resistant, high Tg (175º C by DSC) multifunctional epoxy dielectric substrate. This material is formulated to provide the PWB manufacturer and OEM with vastly improved.. |
|||
Specific Heat Capacity | 1.21 - 1.38 J/g-°C | 0.290 - 0.330 BTU/lb-°F | ASTM E1461-92 |
Park Electrochemical Nelco® N4000-6 FC Multifunctional Epoxy Laminate and Prepreg The Nelco® N4000-6 FC is a high-Tg epoxy laminate and prepreg system that provides a wide range of performance versatility and ease of processing for demanding high-layer count applications.Key Fea.. |
|||
Specific Heat Capacity | 1.21 - 1.38 J/g-°C | 0.290 - 0.330 BTU/lb-°F | ASTM E1461-92 |
Park Electrochemical Nelco® N4000-11 Multifunctional Epoxy Laminate and Prepreg The Nelco® N4000-11 is a CAF resistant, high Tg (175º C by DSC) multifunctional epoxy dielectric substrate. This material is formulated to provide the PWB manufacturer and OEM with vastly improved.. |