Thermal Properties Metric English Comments
Specific Heat Capacity 1.48 J/g-°C
0.354 BTU/lb-°F
Trelleborg Emerson & Cuming Eccolite® Composite Materials Ultra Syntactic Foam
Eccolite Ultra syntactic foam plug assist materials a new engineered thermoplastic compound incorporating Eccospheres, glass microspheres. It is one of the toughest materials designed for the therm..
Specific Heat Capacity 1.48 J/g-°C
0.354 BTU/lb-°F
Azoty Tarnow™ TARNOFORM 300 HI2 POM
Rubber modified grade with very high impact strength and damping capacity.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A.
Specific Heat Capacity 1.48 J/g-°C
0.354 BTU/lb-°F
Azoty Tarnow™ TARNOFORM 300 HI4 POM
High impact strength grade, high damping capacity.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A.
Specific Heat Capacity 1.48 J/g-°C
0.354 BTU/lb-°F
Azoty Tarnow™ TARNOFORM 300 K POM
Tribological modified grade with addition of special chalk, which causes decrease of wear.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A.
Specific Heat Capacity 1.48 J/g-°C
0.354 BTU/lb-°F
Azoty Tarnow™ TARNOFORM 300 LS POM
Injection molding grade based on Tarnoform 300 modified with soluble light stabilizers improving weathering stability.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A.
Specific Heat Capacity 1.48 J/g-°C
0.354 BTU/lb-°F
Azoty Tarnow™ TARNOFORM 300 POM
Basic, fast cycling injection molding grade suitable for many applications.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A.
Specific Heat Capacity 1.48 J/g-°C
0.354 BTU/lb-°F
Azoty Tarnow™ TARNOFORM 300 SI POM
Tribological modified grade with silicon, for better sliding properties in plastic-plastic contact.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A.
Specific Heat Capacity 1.48 J/g-°C
0.354 BTU/lb-°F
Azoty Tarnow™ TARNOFORM 300 TF POM
Tribological modified grade low level addition of PTFE, which lower coefficient of friction and wear.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A.
Specific Heat Capacity 1.48 J/g-°C
0.354 BTU/lb-°F
Azoty Tarnow™ TARNOFORM 300 TF2 POM
Tribological modified grade with addition of 10% PTFE, which causes decreased coefficient of friction and wear.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A.
Specific Heat Capacity 1.48 J/g-°C
0.354 BTU/lb-°F
Azoty Tarnow™ TARNOFORM 300 TF4 POM
Tribological modified grade with addition of 20% PTFE, with very low coefficient of friction and wear.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A.
Specific Heat Capacity 1.48 J/g-°C
0.354 BTU/lb-°F
Azoty Tarnow™ TARNOFORM 300 UV POM
Injection molding grade based on Tarnoform 300 modified with carbon black giving best weathering stability.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A.
Specific Heat Capacity 1.48 J/g-°C
0.354 BTU/lb-°F
Azoty Tarnow™ TARNOFORM 400 LS POM
Injection molding grade based on Tarnoform 400 modified with soluble light stabilizers improving weathering stability.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A.
Specific Heat Capacity 1.48 J/g-°C
0.354 BTU/lb-°F
Azoty Tarnow™ TARNOFORM 400 POM
Easy flowing, fast cycling injection molding grade for manufacturing of thin-wall detailsInformation provided by Zakłady Azotowe w Tarnowie-Moscicach S.A.
Specific Heat Capacity 1.48 J/g-°C
0.354 BTU/lb-°F
Azoty Tarnow™ TARNOFORM 411 POM
Easy flowing, internally strengthened grade for injection molding of thin walled parts of very high mechanical requirements.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A.
Specific Heat Capacity 1.48 J/g-°C
0.354 BTU/lb-°F
Azoty Tarnow™ TARNOFORM 500 HI4 POM
Easy flow high impact grade, possessing also high damping capacityInformation provided by Zakłady Azotowe w Tarnowie-Moscicach S.A.
Specific Heat Capacity 1.48 J/g-°C
0.354 BTU/lb-°F
Azoty Tarnow™ TARNOFORM 500 LS POM
High flow injection molding grade based on Tarnoform 500 modified with soluble light stabilizers improving weathering stability.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A.
Specific Heat Capacity 1.48 J/g-°C
0.354 BTU/lb-°F
Azoty Tarnow™ TARNOFORM 500 POM
Easy flowing grade for injection molding of thin-walled parts or in case of long flow path.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A.
Specific Heat Capacity 1.48 J/g-°C
0.354 BTU/lb-°F
Azoty Tarnow™ TARNOFORM 500 UV POM
High flow injection molding grade based on Tarnoform 500 modified with carbon black giving best weathering stability.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A.
Specific Heat Capacity 1.48 J/g-°C
0.354 BTU/lb-°F
Azoty Tarnow™ TARNOFORM 700 POM
Easy flowing grade for injection molding of thin-walled parts or in case of long flow path.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A.
Specific Heat Capacity 1.48 J/g-°C
0.354 BTU/lb-°F
Azoty Tarnow™ TARNOFORM 200 HI4 POM
Rubber modified grade with very high impact strength and damping capacity.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A.
Specific Heat Capacity 1.48 J/g-°C
0.354 BTU/lb-°F
Azoty Tarnow™ TARNOFORM 200 LS POM
Injection molding grade based on Tarnoform 200 modified with soluble light stabilizers improving weathering stability.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A.
Specific Heat Capacity 1.48 J/g-°C
0.354 BTU/lb-°F
Azoty Tarnow™ TARNOFORM 200 POM
This material is a standard extrusion grade, also could be used for injection molding of low shape complexity details.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A.
Specific Heat Capacity 1.48 J/g-°C
0.354 BTU/lb-°F
Azoty Tarnow™ TARNOFORM 300 HI6 POM
Rubber modified grade with very high impact strength and damping capacity.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A.
Specific Heat Capacity 1.48 J/g-°C
0.354 BTU/lb-°F
Average value: 1.48 J/g-°C Grade Count:3
Overview of materials for Acetal Copolymer, PTFE Filled
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, PTFE Filled". Each property range of values reported is minimum and maximum values of ..
Specific Heat Capacity 1.48 J/g-°C
0.354 BTU/lb-°F
Azoty Tarnow™ TARNOFORM 300 DW POM
Tribological modified grade with combination of damping and wear reducing additives. Finished parts have low coefficient of friction and wear with reduction of acoustic emission during sliding.Infor..
Specific Heat Capacity 1.48 J/g-°C
0.354 BTU/lb-°F
Average value: 1.48 J/g-°C Grade Count:5