Polymer Property : Specific Heat Capacity = 1.77 J/g-°C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Specific Heat Capacity 1.77 J/g-°C
0.423 BTU/lb-°F
Styron CALIBREâ„¢ IM 401 18 Polycarbonate, Impact Modified
CALIBRE® IM401 series resins are impact modified, UL listed polycarbonate resins which contain mold release. CALIBRE IM 401 polycarbonate resins exhibit an excellent balance of impact strength an..