Thermal Properties | Metric | English | Comments |
---|---|---|---|
Specific Heat Capacity | 1.958 J/g-°C | 0.4680 BTU/lb-°F | Melt |
BASF Ultramid® 8333G HI 33% Glass Filled PA6 (Conditioned) Ultramid 8333G HI is a 14% glass reinforced, impact modified PA6 injection molding compound developed for applications requiring improved dry as molded toughness in combination with a
balance of st.. |
|||
Specific Heat Capacity | 1.958 J/g-°C | 0.4680 BTU/lb-°F | Melt |
BASF Ultramid® 8333G HI 33% Glass Filled PA6 (Dry) Ultramid 8333G HI is a 14% glass reinforced, impact modified PA6 injection molding compound developed for applications requiring improved dry as molded toughness in combination with a
balance of st.. |