Polymer Property : Specific Heat Capacity = 2.03 J/g-°C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Specific Heat Capacity 1.80 - 2.03 J/g-°C
0.430 - 0.485 BTU/lb-°F
Average value: 1.91 J/g-°C Grade Count:9
Overview of materials for High Density Polyethylene (HDPE), Crosslinkable
This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Crosslinkable". Each property range of values reported is minimum and ..