Thermal Properties Metric English Comments
Specific Heat Capacity 2.20 J/g-°C
0.526 BTU/lb-°F
DSC
Victrex® PEEK 600G Polyetheretherketone  (discontinued **)
Product Description: High performance thermoplastic material, unreinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection moulding and extrusion, low viscosity, FDA food conta..
Specific Heat Capacity 2.20 J/g-°C

@Temperature 23.0 °C
0.526 BTU/lb-°F

@Temperature 73.4 °F
DSC
Victrex® PEEK 150G903 Black Polyetheretherketone, Unreinforced
Product Description:High performance thermoplastic material, unreinforced Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding, easy flow, FDA food contact compliant, colou..
Specific Heat Capacity 2.20 J/g-°C
0.526 BTU/lb-°F
Average value: 2.20 J/g-°C Grade Count:4
Overview of materials for Acrylonitrile Butadiene Styrene (ABS)/Nylon Blend
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS)/Nylon Blend". Each property range of values reported is minimum an..
Specific Heat Capacity 2.20 J/g-°C
0.526 BTU/lb-°F
Melt
Ineos ABS Triax® 1120 ABS + Polyamide Blend (Conditioned)
Key Features:UnfilledPlatableHigh impact or high impact modifiedSuitable processing methods:Injection moldingFilm extrusionBlow molding
Specific Heat Capacity 2.20 J/g-°C
0.526 BTU/lb-°F
Melt
Ineos ABS Triax® 1120 ABS + Polyamide Blend (DAM)
Key Features:UnfilledPlatableHigh impact or high impact modifiedSuitable processing methods:Injection moldingFilm extrusionBlow molding
Specific Heat Capacity 2.20 J/g-°C
0.526 BTU/lb-°F
Melt
Ineos ABS Triax® KU 2-3050 ABS + Polyamide Blend (Conditioned)
Key Features:UnfilledHigh impact or high impact modifiedLight stabilized or stable to lightHeat stabilized or stable to heatSuitable processing methods:Injection molding
Specific Heat Capacity 2.20 J/g-°C
0.526 BTU/lb-°F
Melt
Ineos ABS Triax® KU 2-3050 ABS + Polyamide Blend (DAM)
Key Features:UnfilledHigh impact or high impact modifiedLight stabilized or stable to lightHeat stabilized or stable to heatSuitable processing methods:Injection molding
Specific Heat Capacity 2.20 J/g-°C

@Temperature 280 °C
0.526 BTU/lb-°F

@Temperature 536 °F
DSC
Eastman Eastar A150 Copolyester, Film
Eastar A150 Copolyester is a poly(1,4-cyclohexylene-dimethylene terephthalate/isophthalate). It is produced by reacting terephthalic acid and isophthalic acid with the glycol 1,4-cyclohexanedimethan..
Specific Heat Capacity 2.20 J/g-°C
0.526 BTU/lb-°F
DuPont Performance Polymers Zytel® 80G33L NC010 Nylon 66  (Unverified Data**)
33% Glass Reinforced Toughened Polyamide 66 Zytel 80G33L NC010 is a 33% glass fiber reinforced polyamide 66 resin with outstanding impact resistance developed using DuPont Super Tough technology.Inf..
Specific Heat Capacity 2.20 J/g-°C
0.526 BTU/lb-°F
DSC
Victrex® HT™ G45 Polyetherketone
Product Description: High performance thermoplastic material, unreinforced PolyEtherKetone (PEK), semi crystalline, depth filtered granules for injection moulding, low flow, FDA food contact complia..
Specific Heat Capacity 2.20 J/g-°C
0.526 BTU/lb-°F
Americas Styrenics Styron® 425 High Impact Polystyrene  (discontinued **)
STYRON® 425 impact polystyrene resin is typically used in thin section parts, hot drink cups and cassettes. It offers heat resistance, easy flow, fast cycling, and excellent tensile and flex proper..