Specific Heat Capacity 2.35 J/g-°C
0.562 BTU/lb-°F
Melt value
BASF Capron® 5233G HS BK-102 33% Glass-Filled Nylon 66 (Dry)  (discontinued **)
Capron 5233G HS BK-102 is a 35% glass reinforced, heat stabilized, pigmented black nylon 6,6 injection molding compound offering excellent strength, rigidity, stiffness, creep resistance, and dimens..