Thermal Properties Metric English Comments
Specific Heat Capacity 2.40 J/g-°C
0.574 BTU/lb-°F
Average value: 2.40 J/g-°C Grade Count:15
Overview of materials for Ethylene Vinyl Alcohol (EVOH)
This property data is a summary of similar materials in the MatWeb database for the category "Ethylene Vinyl Alcohol". Each property range of values reported is minimum and maximum values of appropr..
Specific Heat Capacity 2.40 J/g-°C
0.574 BTU/lb-°F
EVALCA EVAL® LC-L101A Ethylene Vinyl Alcohol Copolymer Resin  (discontinued **)
27 mol % Ethylene.Data provided by EVALCA. Applications: Blown film, melt phase forming. Highest gas barrier EVOH available. EVOH is used in packaging applications because of its outstanding gas ..
Specific Heat Capacity 2.40 J/g-°C
0.574 BTU/lb-°F
EVALCA EVAL® F100 Ethylene Vinyl Alcohol Copolymer Resin  (discontinued **)
32 mol % Ethylene.Data provided by EVALCA. Applications: Melt phase forming. EVOH is used in packaging applications because of its outstanding gas barrier properties.EVAL™ is now produced as a pa..
Specific Heat Capacity 2.40 J/g-°C
0.574 BTU/lb-°F
EVALCA EVAL® LC-F101BZ Ethylene Vinyl Alcohol Copolymer Resin  (discontinued **)
32 mol % Ethylene.Data provided by EVALCA. Applications: Blown film, cast film, melt phase forming, blow molding, profile coextrusion. EVOH is used in packaging applications because of its outstan..
Specific Heat Capacity 2.40 J/g-°C
0.574 BTU/lb-°F
EVALCA EVAL® EP-F104BW Ethylene Vinyl Alcohol Copolymer Resin  (discontinued **)
32 mol % Ethylene.Data provided by EVALCA. Applications: Cast film, blow molding, tubes, coex coating. EVOH is used in packaging applications because of its outstanding gas barrier properties.EVAL..
Specific Heat Capacity 2.40 J/g-°C
0.574 BTU/lb-°F
Estimated by MatWeb from similar grades
EVALCA EVAL® EP-J102B Ethylene Vinyl Alcohol Copolymer Resin  (discontinued **)
32 mol % Ethylene.Data provided by EVALCA. Designed to provide a wide thermoforming range together with high barrier properties. EVAL® EP-J102B is specifically designed for thermoforming applicat..
Specific Heat Capacity 2.40 J/g-°C
0.574 BTU/lb-°F
EVALCA EVAL® LC-H101BD Ethylene Vinyl Alcohol Copolymer Resin  (discontinued **)
38 mol % Ethylene.Data provided by EVALCA. Applications: Blown film. EVOH is used in packaging applications because of its outstanding gas barrier properties.EVAL™ is now produced as a part of th..
Specific Heat Capacity 2.40 J/g-°C
0.574 BTU/lb-°F
EVALCA EVAL® K102 Ethylene Vinyl Alcohol Copolymer Resin  (discontinued **)
38 mol % Ethylene.Data provided by EVALCA. Applications: Solid phase pressure forming. EVOH is used in packaging applications because of its outstanding gas barrier properties.EVAL™ is now produc..
Specific Heat Capacity 2.40 J/g-°C
0.574 BTU/lb-°F
EVALCA EVAL® LC-E105A Ethylene Vinyl Alcohol Copolymer Resin  (discontinued **)
44 mol % Ethylene.Data provided by EVALCA. Applications: Cast film, melt phase forming, solid phase pressure forming, tubes, coex coating. EVOH is used in packaging applications because of its out..
Specific Heat Capacity 2.40 J/g-°C
0.574 BTU/lb-°F
EVALCA EVAL® LC-E151B Ethylene Vinyl Alcohol Copolymer Resin  (discontinued **)
44 mol % Ethylene.Data provided by EVALCA. Applications: Melt phase forming, solid phase pressure forming, blow molding, tubes EVOH is used in packaging applications because of its outstanding gas..
Specific Heat Capacity 2.40 J/g-°C
0.574 BTU/lb-°F
EVALCA EVAL® G156A Ethylene Vinyl Alcohol Copolymer Resin  (discontinued **)
48 mol % Ethylene.Data provided by EVALCA. Applications: Cast film, specialty applications. EVOH is used in packaging applications because of its outstanding gas barrier properties.EVAL™ is now p..
Specific Heat Capacity 2.40 J/g-°C
0.574 BTU/lb-°F
Estimated by MatWeb from similar grades
EVALCA EVAL® G110 Ethylene Vinyl Alcohol Copolymer Resin  (discontinued **)
48 mol % Ethylene.Data provided by EVALCA. EVOH is used in packaging applications because of its outstanding gas barrier properties.EVAL™ is now produced as a part of the Kuraray product line.
Specific Heat Capacity 2.40 J/g-°C
0.574 BTU/lb-°F
Estimated by MatWeb from similar grades
EVALCA EVAL® EF-XL Ethylene Vinyl Alcohol Copolymer Film  (discontinued **)
Biaxially oriented type film; property values for 15 µm film.Data provided by EVALCA. EVOH is used in packaging applications because of its outstanding gas barrier properties.EVAL™ is now produ..
Specific Heat Capacity 2.40 J/g-°C
0.574 BTU/lb-°F
Estimated by MatWeb from similar grades
EVALCA EVAL® EF-F Ethylene Vinyl Alcohol Copolymer Film  (discontinued **)
32 mol % Ethylene. Non oriented type film; property values for 15 µm film.Data provided by EVALCA. Applications: EVOH is used in packaging applications because of its outstanding gas barrier pro..
Specific Heat Capacity 2.40 J/g-°C
0.574 BTU/lb-°F
Estimated by MatWeb from similar grades
EVALCA EVAL® LC-T101 Ethylene Vinyl Alcohol Copolymer Resin  (discontinued **)
32 mol % Ethylene.Data provided by EVALCA. Applications: Solid phase pressure forming. EVOH is used in packaging applications because of its outstanding gas barrier properties.EVAL™ is now produc..
Specific Heat Capacity 2.40 J/g-°C
0.574 BTU/lb-°F
Estimated by MatWeb from similar grades
EVALCA EVAL® EF-E Ethylene Vinyl Alcohol Copolymer Film  (discontinued **)
44 mol % Ethylene. Non oriented type film; property values for 20 µm film.Data provided by EVALCA. Applications: EVOH is used in packaging applications because of its outstanding gas barrier pr..