Polymer Property : Specific Heat Capacity = 2.50 J/g-°C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Specific Heat Capacity 2.50 J/g-°C
0.598 BTU/lb-°F
Schwartz Technical Plastics LAMIGAMID® 1200 Cast Polyamide 12, Dry
Application: sprockets, chain-wheels, pulleys, wheels, slide and seal rings, curve disks, etc.Information provided by Schwartz Technical Plastics GmbH