Thermal Properties | Metric | English | Comments |
---|---|---|---|
Specific Heat Capacity | 3.10 J/g-°C @Temperature 200 °C |
0.741 BTU/lb-°F @Temperature 392 °F |
transition; DSC |
Eastman Neostar FN005 Elastomer Neostar FN005 elastomer is a tough, clear, durable copolyester ether. It was designed for use in the profile and automotive markets, but is also used in packaging and tubing applications where tough.. |
|||
Specific Heat Capacity | 3.10 J/g-°C @Temperature 200 °C |
0.741 BTU/lb-°F @Temperature 392 °F |
transition; DSC |
Eastman Neostar FN006 Elastomer Neostar FN006 elastomer is the second in Eastman’s series of tough, clear, durable copolyester ethers. Developed for use in the profile and automotive markets, it can also be used in packaging and .. |
|||
Specific Heat Capacity | 3.10 J/g-°C @Temperature 200 °C |
0.741 BTU/lb-°F @Temperature 392 °F |
transition; DSC |
Eastman Neostar FN007 Elastomer Neostar FN007 elastomer is the third in Eastman’s series of tough, clear, durable copolyester ethers. Though originally designed for use in the profile and automotive markets, this innovative copol.. |