Glass Transition Temp, Tg
-18.1
°C
-0.580
°F
MDSC, postcured
DuPont Performance Polymers VTR 8655 (GBL-S) , VTR 8650 8655/8650 Blend (discontinued **)
FormulationVTR 8655