Polymer Property : Glass Transition Temp, Tg = -103 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Glass Transition Temp, Tg -75.0 °C
-103 °F
3M Scotchcast™ 2131 Flame-Retardant Compound
3M Scotchcast Flame-Retardant Compound 2131 is a two-part polyurethane resin designed to replace the cable jacket when splicing or repairing mine and portable cables. It formulation makes it particu..