Thermal Properties Metric English Comments
Glass Transition Temp, Tg -110 - 200 °C
-166 - 392 °F
Average value: 127 °C Grade Count:7
Overview of materials for Silicone, RTV, Adhesive/Sealant Grade
This property data is a summary of similar materials in the MatWeb database for the category "Silicone, RTV, Adhesive/Sealant Grade". Each property range of values reported is minimum and maximum va..
Glass Transition Temp, Tg -110 - -95.0 °C
-166 - -139 °F
Silicone Property; ASTM D3418
Arlon Thermabond® R36300W008 0.008" (0.203 mm) Uncured Silicone Rubber with PTFE Coated Fiberglass Carrier
Description: Low Outgassing, Thermally Conductive, Electrically Insulating, Thermabond® Bonds without primerRecommended Primers: Dow Corning S2260Design/Construction: Liner: FEP Product: Uncured S..
Glass Transition Temp, Tg -110 - -95.0 °C
-166 - -139 °F
Silicone Property; ASTM D3418
Arlon Thermabond® R36300W015 0.015" (0.381 mm) Uncured Silicone Rubber with PTFE Coated Fiberglass Carrier
Design/Construction: Liner: FEP Product: Uncured Silicone Rubber Carrier: PTFE Coated FiberglassRecommended Primers: Dow Corning S2260Appearance: White silicone gumThis data represents typical val..
Glass Transition Temp, Tg -110 °C
-166 °F
Cured property; Perkin Elmer TMS-2
Aptek 2712-A/B Very low stress silicone adhesive
Very low stress silicone adhesive; -110ºC to 260ºC operating range; Low outgassing/space gradeAPTEK 2712-A/B is a two component, white, very soft, thixotropic, electrically insulative, silicone ad..
Glass Transition Temp, Tg -110 °C
-166 °F
3M Novec™ 1720 Electronic Grade Coating
3M™ Novec™ 1720 Electronic Grade Coating adds easy clean capabilities to surfaces such as glass flat panel displays and mobile electronic device components. It is a clear, 0.1 wt% fluorosilane pol..