Thermal Properties Metric English Comments
Glass Transition Temp, Tg -28.9 °C
-20.0 °F
HR 10 K/min, half height
Styron Sprintan® SLR 4630 Solution Styrene Butadiene Rubber (S-SBR)
Composition: SPRINTAN® SLR-4630 – Schkopau is manufactured by anionic solution polymerization using an organo-lithium initiator. In relation to solid rubber the grade is extended with 37.5 p..
Glass Transition Temp, Tg -28.9 °C
-20.0 °F
HR 10 K/min; half height; DSC
Dow SE SLR-4630 Solution polymerized Styrene Butadiene Rubber (S-SBR)
SE SLR-4630 is manufactured by anionic solution polymerization using lithium initiator and is extended with 37.5 parts of TDAE oil in relation to solid rubber. It is a product with medium styrene a..