Thermal Properties Metric English Comments
Glass Transition Temp, Tg -31.6 °C
-24.9 °F
ASTM D3417
REXtac Rextac® RT 5224 Amorphous Polyalphaolefin (APAO)
Modified Bitumen Roofing Grade.Description: High molecular weight REXtac, high ethylene copolymer, and FDA compliantFeatures: High viscosity and low crystallinityApplications: Component of modified ..