Polymer Property : Glass Transition Temp, Tg = -34.6 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Glass Transition Temp, Tg -37.0 °C
-34.6 °F
ASTM D3417
REXtac Rextac® RT 2535 Amorphous Polyalphaolefin (APAO)
Adhesive and Sealant Grade.Description: Ethylene copolymer and FDA compliantFeatures: Low softening point, excellent tack, excellent flexibility, and long open timeApplications: Component of hot mel..
Glass Transition Temp, Tg -37.0 °C
-34.6 °F
ASTM D3417
REXtac Rextac® RT 2585 Amorphous Polyalphaolefin (APAO)
Adhesive and Sealant Grade.Description: Ethylene copolymer and FDA compliantFeatures: Low softening point, excellent tack, excellent flexibility, long open time, and high viscosityApplications: Comp..
Glass Transition Temp, Tg -37.0 °C
-34.6 °F
ASTM D3417
REXtac Rextac® RT 3535 Amorphous Polyalphaolefin (APAO)
Modified Bitumen Roofing Grade.Description: Ethylene copolymer and FDA compliantFeatures: Excellent low temperature flexibilityApplications: Component of modified bitumen roofing systemsOther Proper..
Glass Transition Temp, Tg -37.0 °C
-34.6 °F
Dow Pellethane® 2102-85A Polyurethane Elastomer, Polyester Polycaprolactone Based  (discontinued **)
PELLETHANE® 2102-85A elastomer is a polyester polycaprolactone based polyurethane elastomer which combines excellent resistance to fuels and oils with enhanced UV stability and good hydrolytic stab..
Glass Transition Temp, Tg -37.0 °C
-34.6 °F
DSC
Lubrizol ESTANE® 58245 Ether Based Thermoplastic Polyurethane
Features: High moisture vapor transmission. Good low temperature properties and elasticity.Uses: Blown and flat die/cast film extrusion.Available in Americas, Europe, Middle East, Africa, India and ..
Glass Transition Temp, Tg -37.0 °C
-34.6 °F
DSC
Lubrizol Estane® 2355-80AE Thermoplastic Polyurethane Elastomer
Formerly PellethaneFeature: Damping capacityAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Pellethane product line from Dow in 2009...
Glass Transition Temp, Tg -37.0 °C
-34.6 °F
ASTM D3417
REXtac Rextac® RT 3585 Amorphous Polyalphaolefin (APAO)
Modified Bitumen Roofing Grade.Description: Ethylene copolymer and FDA compliantFeatures: High melt viscosity and excellent low temperature flexibilityApplications: Component of modified bitumen roo..
Glass Transition Temp, Tg -37.0 °C
-34.6 °F
ASTM D3417
REXtac Rextac® RT 4535 Amorphous Polyalphaolefin (APAO)
Wire and Cable Grade.Description: Ethylene copolymer and FDA compliantFeatures: Excellent low temperature flexibility, moisture barrier and adhesionApplications: Flooding and filling compounds for w..