Thermal Properties | Metric | English | Comments |
---|---|---|---|
Glass Transition Temp, Tg | -39.8 - -33.8 °C | -39.6 - -28.8 °F | Zeon Test #404 |
Zeon Chemicals HyTemp® AR74 AR Polyacrylate Elastomer HyTemp AR74 acrylic elastomer contains one or more acrylic esters with a small percentage of a chlorine reactive cure site. Vulcanizates have excellent oil, heat and compression resistance.Excellent.. |