Thermal Properties | Metric | English | Comments |
---|---|---|---|
Glass Transition Temp, Tg | -20.3 °C | -4.54 °F | ASTM D3417 |
REXtac Rextac® RT 5218 Amorphous Polyalphaolefin (APAO) Modified Bitumen Roofing Grade.Description: High molecular weight REXtac, ethylene copolymer, and FDA compliantFeatures: High viscosity and high ring and ball softening pointApplications: Component .. |