Thermal Properties | Metric | English | Comments |
---|---|---|---|
Glass Transition Temp, Tg | -49.0 °C | -56.2 °F | |
Huntsman KRYSTALFLEX® PE 499 Polyurethane Optical Aliphatic Film Key Properties:Moisture ResistanceChemical CompatibilityCooler ProcessingHigher AdhesionMultiple Design OptionNo special storage requiredInformation provided by Alliance Polymers |
|||
Glass Transition Temp, Tg | -49.0 °C | -56.2 °F | DSC |
Lubrizol ESTANE® 54640 Ether Based Thermoplastic Polyurethane Very good physical properties and hydrolysis resistance and wide processing window for calendering.Uses: Melt coating/calendering, flat die/cast film extrusionAvailable in Americas, Europe, Middle E.. |
|||
Glass Transition Temp, Tg | -49.0 °C | -56.2 °F | ExxonMobil Method |
ExxonMobil Exact™ 9061 Ethylene-based Plastomer Resin Product Description: Exact 9061 plastomer is an ethylene butene copolymer produced using ExxonMobil Chemical's EXXPOL™ Technology, exhibiting both plastic and elastomeric properties.Key Features:P.. |
|||
Glass Transition Temp, Tg | -49.0 °C | -56.2 °F | ExxonMobil Method |
ExxonMobil Exact™ 9071 Ethylene-based Plastomer Resin Product Description: Exact 9071 plastomer is an ethylene butene copolymer produced using ExxonMobil Chemical's EXXPOL™ Technology, exhibiting both plastic and elastomeric properties.Key Features:P.. |
|||
Glass Transition Temp, Tg | -49.0 °C | -56.2 °F | Dow Method |
Dow AMPLIFY™ GR 209 Maleic anhydride grafted (MAH) polymer AMPLIFY™ GR 209 Functional Polymer is a post reactor maliec anhydride grafted (MAH) polymer. The base polymer is an ethylene-butene copolymer exhibiting high flexibility and elasticity. It can be.. |
|||
Glass Transition Temp, Tg | -49.0 °C | -56.2 °F | DSC |
Lubrizol ESTANE® 58311 Ether Based Thermoplastic Polyurethane Features: Very good physical properties, hydrolysis resistance, low temperature performance and abrasion. Wide processing window for extrusion.Uses: Flat Die/Cast Film Extrusion, Profile ExtrusionAv.. |