Thermal Properties Metric English Comments
Glass Transition Temp, Tg -48.9 °C
-56.0 °F
DSC, 10ºC/min; DIN 51.007
Lubrizol Advanced Materials PEARLCOAT® 168K Thermoplastic Polyurethane Elastomer
PEARLCOAT® 168K is a polyether-based TPU, supplied in form of translucent, colorless pellets, offering adequate hardness, excellent low-temperature flexibility and very good hydrolysis resistance..
Glass Transition Temp, Tg -48.9 °C
-56.0 °F
Dow Method
Dow FLEXOMER™ DFDB-1088 NT Very Low Density Polyethylene (VLDPE) Resin
FLEXOMER™ DFDB-1088 NT is an ethylene-butene copolymer produced via gas phase polymerization from Dow. It can be utilized in monolayer and co-extruded films and in blends with other polyolefins to..
Glass Transition Temp, Tg -48.9 °C
-56.0 °F
reported value is for pure FLEXOMER™ DFDB-1088 NT, the primary component in this blend; Dow Method
Dow FLEXOMER™ DFDA-1098 NT Very Low Density Polyethylene (VLDPE) Resin
FLEXOMER™ DFDA-1098 NT is an ethylene-butene copolymer with a unique olefinic composition for improved process-ability and material handling. This product is produced via gas phase polymerization ..