Polymer Property : Glass Transition Temp, Tg = -69.0 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Glass Transition Temp, Tg -69.0 - -17.0 °C
-92.2 - 1.40 °F
Average value: -40.2 °C Grade Count:49
Overview of materials for Thermoplastic Polyurethane, Elastomer, Ether Grade
This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Polyurethane, Elastomer, Ether Grade". Each property range of values reported is minimum a..
Glass Transition Temp, Tg -69.0 °C
-92.2 °F
Lubrizol Estane® 2103-70A Thermoplastic Polyurethane Elastomer
Formerly PellethaneFeature: High MVTRAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Pellethane product line from Dow in 2009.