Glass Transition Temp, Tg -74.0 °C
-101 °F
Cured property; JMTP P200
Aptek 2503R-A/B Premeasured conformal urethane coating repair kit
APTEK 2503-A/B is an unfilled, two component, electrically insulating, transparent, flexible urethane coating system designed for the encapsulation and protection of electrical/electronic components..
Glass Transition Temp, Tg -74.0 °C
-101 °F
Cured property; ASTM E831-86
Aptek 2503-A/B Low modulus urethane conformal coating
APTEK 2503-A/B is an unfilled, two component, electrically insulating, transparent, flexible urethane coating system designed for the encapsulation and protection of electronic services mounted on p..