Glass Transition Temp, Tg 0.400 °C
32.7 °F
Loctite® Output™ 5404 Heat Cure Silicone
Thermally Conductive BondersLoctite® Thermally Conductive Adhesives eliminate the need for mechanical fasteners and clips, while providing the most efficient thermal transfer between transistors or..