Polymer Property : Glass Transition Temp, Tg = 188 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Glass Transition Temp, Tg 188 °C
370 °F
ASTM D4065-01
Premix Premi-Glas® 1265 VE 1265-VE (Compression Molded) Glass Reinforced Vinyl Ester TMC  (discontinued **)<
Description: Premi-Glas® 1265 VE is a glass reinforced vinyl ester molding compound designed for automotive under the hood applications. Key features and benefits: Designed for Injection or Injecti..
Glass Transition Temp, Tg 188 °C
370 °F
ASTM D4065-01
Premix Premi-Glas® 1265 VE 1265-VE (Injection Compression Molded) Glass Reinforced Vinyl Ester TMC  (discontin
Description: Premi-Glas® 1265 VE is a glass reinforced vinyl ester molding compound designed for automotive under the hood applications. Key features and benefits: Designed for Injection or Injecti..
Glass Transition Temp, Tg 188 °C
370 °F
Dry
Hexcel® HexPly® F263 Epoxy Resin
HexPly® F263 is a structural, heat resistant epoxy resin formulated for excellent translation of high modulus carbon fiber properties in typically aerospace applications. HexPly® F263 is a high te..
Glass Transition Temp, Tg 188 °C
370 °F
ASTM D4065-01
Premix Premi-Glas® 1282-32 VE Glass Reinforced Vinyl Ester SMC  (discontinued **)
Description: Premi-Glas® 1282-32 VE SMC is an enhanced high strength glass reinforced vinyl ester molding compound formulated for under-the-hood automotive applications. Key features and benefi..
Glass Transition Temp, Tg 188 °C
370 °F
ASTM D4065-01
Premix Premi-Glas® 1281-32 VE Glass Reinforced Vinyl Ester SMC  (discontinued **)
Description: Premi-Glas® 1281-32 VE SMC is a high strength glass reinforced vinyl ester sheet molding compound formulated for under-the-hood automotive applications. Key features and benefits: Desi..
Glass Transition Temp, Tg 188 °C
370 °F
ISO 6721 DMS
Premix Premi-Glas® 1285VE 1285 VE Glass Reinforced Vinyl Ester SMC  (discontinued **)
Description: Premi-Glas® 1285 VE is a glass reinforced vinyl ester sheet molding compound designed for automotive under the hood applications. Key features and benefits: Designed for compression mo..