Thermal Properties | Metric | English | Comments |
---|---|---|---|
Glass Transition Temp, Tg | 200 °C | 392 °F | ISO 11357 |
Premix Thermoplastics PRETECH Halogen-free Engineering Thermoplastics Halogen-free PRETECH engineering thermoplastics enable environmentally friendly and cost efficient V-0 product solutions with excellent mechanical and electrical properties. PRETECH combines high th.. |
|||
Glass Transition Temp, Tg | 200 °C | 392 °F | TMA; IPC-TM-650.2.4.24c |
Park Electrochemical Nelco® N4000-13 BC® Buried Capacitance™, High-Speed Multifunctional Epoxy Laminate and Prepreg The Nelco N4000-13 series is an enhanced epoxy resin system engineered to provide both outstanding thermal and high signal speed / low signal loss properties. The Nelco N4000-13 BC® is offered as a.. |
|||
Glass Transition Temp, Tg | 200 °C | 392 °F | TMA; IPC-TM-650.2.4.24c |
Park Electrochemical Nelco® N4000-13 EP™ BC® Buried Capacitance™, High-Speed Multifunctional Epoxy Laminate and Prepreg Nelco N4000-13 EP™ is an enhanced epoxy resin system engineered for today’s leadfree requirements where multiple solder reflow at temperatures approaching 260ºC are required. N4000-13 EP provides.. |
|||
Glass Transition Temp, Tg | 200 °C | 392 °F | TMA; IPC-TM-650.2.4.24c |
Park Electrochemical Nelco® N4000-13 High-Speed Multifunctional Epoxy Laminate and Prepreg The Nelco® N4000-13 series is an enhanced epoxy resin system engineered to provide both outstanding thermal and high signal speed / low signal loss properties. N4000-13 SI® is excellent for applic.. |
|||
Glass Transition Temp, Tg | 200 °C | 392 °F | TMA; IPC-TM-650.2.4.24c |
Park Electrochemical Nelco® N4000-13 SI® High-Speed Multifunctional Epoxy Laminate and Prepreg The Nelco® N4000-13 series is an enhanced epoxy resin system engineered to provide both outstanding thermal and high signal speed / low signal loss properties. N4000-13 SI® is excellent for applic.. |
|||
Glass Transition Temp, Tg | 200 °C | 392 °F | TMA; IPC-TM-650.2.4.24c |
Park Electrochemical Nelco® N4350-13 RF Microwave Performance, Modified Epoxy The Nelco N4350-13 RF and N4380-13 RF series are enhanced epoxy resin systems specifically engineered to provide a unique solution for design applications that demand outstanding thermal properties,.. |
|||
Glass Transition Temp, Tg | >= 200 °C | >= 392 °F | |
Humiseal 1C49 Silicone Conformal Coating Humiseal 1C49 Silicone Conformal CoatingHigh temperature resistanceGood dielectrical propertiesGood moisture resistanceRepairableUL ApprovedMIL-I-46058C ApprovedPasses thermal shock test (MIL-I-4605.. |
|||
Glass Transition Temp, Tg | >= 200 °C | >= 392 °F | |
Humiseal 1C51 Silicone Conformal Coating Humiseal 1C51 Silicone Conformal CoatingHigh temperature resistanceGood dielectrical propertiesGood moisture resistanceRepairableUL ApprovedMIL-I-46058C ApprovedPasses thermal shock test (MIL-I-4605.. |
|||
Glass Transition Temp, Tg | >= 200 °C | >= 392 °F | |
Humiseal 1C55 Silicone Conformal Coating Humiseal 1C55 Silicone Conformal CoatingHigh temperature resistanceGood dielectrical propertiesGood moisture resistanceRepairableUL Approval PendingMIL-I-46058C Approval PendingPasses thermal shock .. |
|||
Glass Transition Temp, Tg | >= 200 °C | >= 392 °F | |
Humiseal 1C63 Silicone Conformal Coating Humiseal 1C63 Silicone Conformal CoatingHigh temperature resistanceGood dielectrical propertiesGood moisture resistanceRepairableUL Approval PendingMIL-I-46058C Approval PendingPasses thermal shock .. |
|||
Glass Transition Temp, Tg | >= 200 °C | >= 392 °F | |
Humiseal 1C65 Silicone Conformal Coating Humiseal 1C65 Silicone Conformal CoatingHigh temperature resistanceGood dielectrical propertiesGood moisture resistanceRepairableUL Approval PendingMIL-I-46058C Approval PendingPasses thermal shock .. |
|||
Glass Transition Temp, Tg | 200 °C | 392 °F | Tg |
Industrial Laminates/Norplex P95 Glass Fabric Description: Woven glass fabric with polyimide resin engineered to maintain excellent physical properties at 240°C. Low coefficient of thermal expansion, high mechanical strength.Thickness Tested.. |
|||
Glass Transition Temp, Tg | 200 °C | 392 °F | ISO 11357-2 |
Menzolit Menzolit® SMC 0430 Unsaturated Polyester UP SMC 0430 is a low emission Class-A SMC for on-line painted exterior body applications on passenger cars. These compounds mould to parts with excellent surface quality for on-line painted body panel.. |
|||
Glass Transition Temp, Tg | 200 °C | 392 °F | ISO 11357-2 |
Menzolit Menzolit® SMC 0420 Unsaturated Polyester UP SMC 0420 is a low density Premium Class-A SMC for exterior body applications on cars, LCV´s and trucks. These compounds mould to light weight parts with good up to excellent surface quality for .. |
|||
Glass Transition Temp, Tg | 200 °C | 392 °F | ISO 11357-2 |
Menzolit Menzolit® SMC 0421 Unsaturated Polyester UP SMC 0421 is a low density premium Class-A SMC for on-line painted exterior body applications on cars. These compounds mould to light weight parts with excellent surface quality for on-line painted .. |
|||
Glass Transition Temp, Tg | 200 °C | 392 °F | |
SABIC Innovative Plastics Ultem DT1800E PEI Blend (Asia Pacific) Improved ductility, transparent, standard flow Polyetherimide blend (Tg 200C) with internal mold release and enhanced ductility. ECO Conforming.This data was supplied by SABIC-IP for the Asia Pacifi.. |
|||
Glass Transition Temp, Tg | 200 °C | 392 °F | |
SABIC Innovative Plastics Ultem DT1800E PEI Blend (Europe-Africa-Middle East) Improved ductility, transparent, standard flow Polyetherimide blend (Tg 200C) with internal mold release and enhanced ductility. ECO Conforming.This data was supplied by SABIC-IP for the Europe-Afri.. |
|||
Glass Transition Temp, Tg | 200 °C | 392 °F | |
SABIC Innovative Plastics Ultem DT1810E PEI Blend (Asia Pacific) Improved ductility, transparent, enhanced flow Polyetherimide blend (Tg 200C) with internal mold release and enhanced ductility. ECO Conforming.This data was supplied by SABIC-IP for the Asia Pacifi.. |
|||
Glass Transition Temp, Tg | 200 °C | 392 °F | |
SABIC Innovative Plastics Ultem DT1810E PEI Blend (Europe-Africa-Middle East) Improved ductility, transparent, enhanced flow Polyetherimide blend (Tg 200C) with internal mold release and enhanced ductility. ECO Conforming.This data was supplied by SABIC-IP for the Europe-Afri.. |
|||
Glass Transition Temp, Tg | 200 °C | 392 °F | |
SABIC Innovative Plastics ULTEM DT1810EV PEI Blend Improved ductility, transparent, enhanced flow Polyetherimide blend (Tg 200C) with internal mold release and enhanced ductility. ECO Conforming, UL94 V0 listed. |
|||
Glass Transition Temp, Tg | 200 °C | 392 °F | |
SABIC Innovative Plastics ULTEM DT1810EV PEI Blend (Asia Pacific) Improved ductility, transparent, enhanced flow Polyetherimide blend (Tg 200C) with internal mold release and enhanced ductility. ECO Conforming, UL94 V0 listed. |
|||
Glass Transition Temp, Tg | 200 °C | 392 °F | |
SABIC Innovative Plastics Ultem DT1810EV PEI Blend (Europe-Africa-Middle East) Improved ductility, transparent, enhanced flow Polyetherimide blend (Tg 200C) with internal mold release and enhanced ductility. ECO Conforming, UL94 V0 listed.This data was supplied by SABIC-IP for.. |
|||
Glass Transition Temp, Tg | 200 °C | 392 °F | |
SABIC Innovative Plastics ULTEM EXUM0167 PEI Blend Improved ductility, transparent, standard flow Polyetherimide blend (Tg 200C) with internal mold release and enhanced ductility. ECO Conforming. |
|||
Glass Transition Temp, Tg | 200 °C | 392 °F | |
SABIC Innovative Plastics ULTEM EXUM0169 PEI Blend Improved ductility, transparent, enhanced flow Polyetherimide blend (Tg 200C) with internal mold release and enhanced ductility. ECO Conforming. |
|||
Glass Transition Temp, Tg | 200 °C | 392 °F | Dry; RDS 7700 |
Hexcel® HexPly® 8552 Epoxy Matrix HexPly® 8552 is an amine cured, toughened epoxy resin system supplied with unidirectional or woven carbon or glass fibers. HexPly® 8552 is recommended for structural applications requiring high st.. |
|||
Glass Transition Temp, Tg | 200 °C | 392 °F | Ultimate Tg |
Tra-Con Tra-Bond 77-1S One Component SMD Adhesive TRA-BOND 77-1S one component, solvent-free, insulating epoxy adhesive is designed specifically for attaching surface mounted devices (SMDs) to printed circuit boards prior to wave solder. TRA-BOND 7.. |
|||
Glass Transition Temp, Tg | >= 200 °C | >= 392 °F | Cure 150ºC/1 hour + 275ºC/1 hours; Ramp 20°C/min to 350ºC |
Epoxy Technology EPO-TEK® TV1002 Polyimide Adhesive Material Description: A single component, screen printable polyimide adhesive designed for semiconductor wafer passivation applications. It is a high temperature chemistry capable of resisting >400.. |
|||
Glass Transition Temp, Tg | 200 °C | 392 °F | TMA; IPC TM-650 2.4.24 |
Arlon 38N High Performance Polyimide Low-Flow 38N is an improved polyimide low-flow prepreg suitable for bonding multilayer polyimide rigid-flex, attaching heat sinks to polyimide MLBs, or other applications where minimal and uniform resin flow.. |
|||
Glass Transition Temp, Tg | >= 200 °C | >= 392 °F | |
Bulk Molding Compounds BMC 940 Vinyl Ester Bipolar Plate Material Bulk Molding Compounds, Inc. is the largest manufacturer of thermoset bulk molding compounds in North America, serving the automotive, appliance, and electrical markets. BMC thermosets are the most .. |