Thermal Properties Metric English Comments
Glass Transition Temp, Tg 98.0 °C
208 °F
TM R050-25
Resinlab® EP1320LV Heat Cure Epoxy Conformal Coating
Resinlab™ EP1320 and EP1320LV are one part heat cure epoxy conformal coatings. They can also be used as a small mass potting compounds, structural adhesives, or insulating polymer systems where the..
Glass Transition Temp, Tg 98.0 °C
208 °F
Eastman Tenite 264-16 CAB Cellulose Acetate Butyrate  (discontinued **)
16% Plasticized. ISO data as provided by the manufacturer, Eastman Chemical.
Glass Transition Temp, Tg 98.0 °C
208 °F
Lucite International Elvacite ® 2010 Acrylic Resin
Elvacite® 2010 is a medium molecular weight methyl methacrylate polymer. 2010 is excellent for use as a general purpose grade for lacquer coatings, such as barrier topcoats for vinyl. It provides..
Glass Transition Temp, Tg 98.0 °C
208 °F
Ultimate Tg
Tra-Con Tra-Bond 293-1 General Purpose Instrument Epoxy Adhesive
TRA-BOND 293-1 general purpose epoxy adhesive is designed to provide strong, resilient bonds to a variety of difficult-to-bond substrates, such as gold, nickel, silver, copper, and brass. The 293-se..
Glass Transition Temp, Tg 98.0 °C
208 °F
Ultimate Tg
Tra-Con Tra-Bond 293-1M General Purpose Instrument Epoxy Adhesive
TRA-BOND 293-1M general purpose epoxy adhesive is designed to provide strong, resilient bonds to a variety of difficult-to-bond substrates, such as gold, nickel, silver, copper and brass. The 293-se..
Glass Transition Temp, Tg 98.0 °C
208 °F
Armstrong C-7/H20 Epoxy Adhesive
A clear, unfilled, medium viscosity adhesive recommended for use with any Armstrong Activator. Physical property data included covers C-7 used with Activators W and H-20. All other Activators may ..
Glass Transition Temp, Tg 98.0 °C
208 °F
Armstrong A-3/E Epoxy Adhesive
A Jet black epoxy paste especially formulated for bonding rigid materials. When used with Activator A or E, A-3 exhibits excellent bonding properties to phenolics, precious stones, ceramics, glass,..
Glass Transition Temp, Tg 98.0 - 107 °C
208 - 225 °F
Average value: 102 °C Grade Count:3
Overview of materials for Cellulose Acetate Butyrate, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Cellulose Acetate Butyrate, Molded". Each property range of values reported is minimum and maximum value..