Thermal Properties | Metric | English | Comments |
---|---|---|---|
Glass Transition Temp, Tg | 102 - 122 °C | 216 - 252 °F | Average value: 110 °C Grade Count:21 |
Overview of materials for Acrylic, General Purpose, Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, General Purpose, Molded". Each property range of values reported is minimum and maximum values .. |
|||
Glass Transition Temp, Tg | 102 °C | 216 °F | ASTM D3418 |
Kolon DIAMAT® IH Description: DIAMAT® is a specially formulated high impact grade PMMA resin from KOLON. The acrylic composition results in an excellent balance of impact resistance and high modulus at reasonabl.. |
|||
Glass Transition Temp, Tg | 102 °C | 216 °F | |
Lucite International Elvacite ® 3008 Acrylic Resin Elvacite® 3008 is a medium viscosity, methyl methacrylate based bead resin specially designed for use in plastic and vinyl coatings and inks.Information provided by Lucite International |
|||
Glass Transition Temp, Tg | 102 °C | 216 °F | |
Lucite International Elvacite ® 3010 Acrylic Resin Elvacite® 3010 is a medium viscosity, methyl methacrylate based bead resin specially designed for use in plastic and vinyl coatings and inks.Information provided by Lucite International |
|||
Glass Transition Temp, Tg | 102 °C | 216 °F | JIS K7121 |
Zeon Chemicals Zeonor® 1020R Cyclo Olefin Polymer Zeonor® is a line of thermoplastic polyolefin resin with an excellent combination of optical and electronic properties. These unique Cyclo Olefin Polymer (COP) was developed by Zeon Corporation usi.. |
|||
Glass Transition Temp, Tg | 102 °C | 216 °F | Ultimate Tg |
Tra-Con Tra-Bond 526H02 Information provided by Tra-Con Inc. |
|||
Glass Transition Temp, Tg | 102 °C | 216 °F | Ultimate Tg |
Tra-Con Tra-Bond F112 Fiber Optic Epoxy Adhesive TRA-BOND F112 is a long pot life, impact resistant, fiber-optic adhesive. This two-part, low viscosity epoxy has the distinct advantage of remaining below 3000 cps for a minimum of 40 minutes. This .. |
|||
Glass Transition Temp, Tg | 102 °C | 216 °F | |
Atom Adhesives AA-BOND F112 Epoxy Adhesive AA-BOND F112 is an impact resistant, fiber-optic adhesive. AA-BOND F112 is two-part, low viscosity epoxy has the distinct advantage of remaining below 3000 cps for a minimum of 40 minutes. AA-BOND F.. |
|||
Glass Transition Temp, Tg | 102 °C | 216 °F | |
Eastman Tenite 525-10 CAB Cellulose Acetate Butyrate
(discontinued **) 10% Plasticized. ISO data as provided by the manufacturer, Eastman Chemical. |