Polymer Property : Glass Transition Temp, Tg = 22.0 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Glass Transition Temp, Tg 22.0 - 60.0 °C
71.6 - 140 °F
Average value: 43.0 °C Grade Count:4
Overview of materials for Polybutylene Terephthalate (PBT), 40% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), 40% Glass Fiber Filled". Specific grades with glass content between 35..
Glass Transition Temp, Tg 22.0 °C
71.6 °F
Mallard Creek Polymers ROVENE® 4021 SBR Latex
ROVENE® 4021 is a “self” cross-linking, carboxylated styrene-butadiene emulsion that has a firm hand with outstanding strength properties. This binder is especially suited for various n..
Glass Transition Temp, Tg 22.0 °C
71.6 °F
Styron XZ 97217.00 Styrene Acrylate
Performance Features: For use in D1 building adhesive formulationsApplications: Waterproofing Membranes and MasticsEuropeInformation provided by Styron
Glass Transition Temp, Tg 22.0 °C
71.6 °F
Ultimate Tg
Tra-Con Tra-Coat CF103B UV Curable Rigid Coating
TRA-COAT CF103B is a high-gloss, UV curable polymer coating. It provides a wear layer with outstanding gloss retention, moisture resistance, stain resistance, and abrasion resistance. It can be used..
Glass Transition Temp, Tg 22.0 °C
71.6 °F
dynamic; DIN 53 736
Hippe PBT GF 30 Polybutylene Terephthalate 30% Glass fiber Reinforced
PBT GF is a highly versatile, semi-crystalline structural thermoplastic reinforced with 30% glass fiber, with very high rigidity and strength characteristics and excellent electrical insulation prop..
Glass Transition Temp, Tg 22.0 °C
71.6 °F
dynamic; DIN 53 736
Hippe PBT Polybutylene Terephthalate
The mechanical properties of PBT are generally inferior to the partially crystallized PET, however, PBT is more easily machined.Information provided by Hippe.