Polymer Property : Glass Transition Temp, Tg = 239 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Glass Transition Temp, Tg 42.0 - 115 °C
108 - 239 °F
Average value: 73.8 °C Grade Count:6
Overview of materials for Epoxy Adhesive, Flexible
This property data is a summary of similar materials in the MatWeb database for the category "Epoxy Adhesive, Flexible". Each property range of values reported is minimum and maximum values of appro..