Thermal Properties | Metric | English | Comments |
---|---|---|---|
Glass Transition Temp, Tg | 24.0 °C | 75.2 °F | |
Mallard Creek Polymers Rovene® 4045 Styrene-Butadiene Emulsion Description: Rovene® 4045 is recommended in applications where soil and aggregate stabilization and binding are required. Rovene® 4045 can be used in the process of road construction, landscap.. |
|||
Glass Transition Temp, Tg | 24.0 °C | 75.2 °F | |
Mallard Creek Polymers Tykote® 1005 Styrene-Butadiene Emulsion Regulartory StatusFDA components in food contact applications.176.170 components of paper and paperboard in contact with aqueous and fatty foods176.180 components of paper and paperboard in contact .. |
|||
Glass Transition Temp, Tg | 24.0 °C | 75.2 °F | |
Styron DL 399 Carboxylated SB Performance Features: Medium hard tough filmApplications: Thermo MoldableEuropeInformation provided by Styron |
|||
Glass Transition Temp, Tg | 24.0 °C | 75.2 °F | |
Styron DL 280NA Styrene Acrylate Performance Features: Excellent adhesion and strength, film clarity, filler toleranceApplications: MasticsNorth AmericaInformation provided by Styron |
|||
Glass Transition Temp, Tg | 24.0 °C | 75.2 °F | |
Styron DL 280NA Styrene Acrylate Performance Features: Light stable, wet-room adhesive, non-yellowing, heat sealableApplications: Heat Sealable and Laminated (Metalized Paper)North AmericaInformation provided by Styron |