Thermal Properties Metric English Comments
Glass Transition Temp, Tg 124 °C
255 °F
Ultimate Tg
Tra-Con Tra-Bond 933-1 Moisture Resistant Chip Encapsulant
TRA-BOND 933-1 one component, highly filled, electrically insulating epoxy encapsulant is designed for encapsulating microelectronic chips. This epoxy provides excellent environmental and mechanical..
Glass Transition Temp, Tg 124 °C
255 °F
Dry
Hexcel® HexPly® F515 Epoxy Resin
HexPly® F515 is an advanced, industrial grade, modified epoxy formulation designed for either vacuum bag or autoclave curing to offer very high laminate strengths, coupled with increased fracture t..