Thermal Properties | Metric | English | Comments |
---|---|---|---|
Glass Transition Temp, Tg | -3.00 °C | 26.6 °F | DSC |
Lubrizol ESTANE® 5707 Ester Based Thermoplastic Polyurethane Features: Very high tensile strength, excellent low temperature flexibility and superior abrasion and cut resistance. It is processed by means of solution coating, extrusion and melt coating.Uses: S.. |
|||
Glass Transition Temp, Tg | -3.00 °C | 26.6 °F | DSC |
Eastman Eastman AP005 Copolyester Applications:Automotive componentsBreathable filmsElectrical/electronic componentsFilm ModificationFlexible hingesHose mandrelIndustrial componentsIndustrial hoses/beltsOffice furniturePackagingPoly.. |
|||
Glass Transition Temp, Tg | -3.00 °C | 26.6 °F | DSC |
Eastman Eastman AP006 Copolyester Applications:Automotive componentsBreathable filmsElectrical/electronic componentsFilm ModificationFlexible hingesHose mandrelIndustrial componentsIndustrial hoses/beltsOffice furniturePackagingPoly.. |
|||
Glass Transition Temp, Tg | -3.00 °C | 26.6 °F | DSC |
Eastman Eastman AP007 Copolyester Applications:Automotive componentsBreathable filmsElectronic componentsFilm ModificationFlexible hingesHose mandrelIndustrial componentsOffice furniturePackagingPolymer modificationProfilesRubber an.. |
|||
Glass Transition Temp, Tg | -3.00 °C | 26.6 °F | |
Eastman Ecdel PCCE 9965 Copolyester Ether Elastomer ISO data as provided by the manufacturer, Eastman Chemical |
|||
Glass Transition Temp, Tg | -3.00 °C | 26.6 °F | |
Eastman Ecdel PCCE 9967 Copolyester Ether Elastomer ISO data as provided by the manufacturer, Eastman Chemical |
|||
Glass Transition Temp, Tg | -3.00 °C | 26.6 °F | DSC |
Eastman Neostar FN005 Elastomer Neostar FN005 elastomer is a tough, clear, durable copolyester ether. It was designed for use in the profile and automotive markets, but is also used in packaging and tubing applications where tough.. |
|||
Glass Transition Temp, Tg | -3.00 °C | 26.6 °F | DSC |
Eastman Neostar FN006 Elastomer Neostar FN006 elastomer is the second in Eastman’s series of tough, clear, durable copolyester ethers. Developed for use in the profile and automotive markets, it can also be used in packaging and .. |
|||
Glass Transition Temp, Tg | -3.00 °C | 26.6 °F | DSC |
Eastman Neostar FN007 Elastomer Neostar FN007 elastomer is the third in Eastman’s series of tough, clear, durable copolyester ethers. Though originally designed for use in the profile and automotive markets, this innovative copol.. |
|||
Glass Transition Temp, Tg | -3.00 °C | 26.6 °F | |
Asahi Glass AFLAS® 100H TFE/P Fluoroelastomer AFLAS® 100/150 fluoroelastomers are alternating copolymers of tetrafluoroethylene and propylene. They offer 1) excellent heat resistance, 2) exceptional chemical resistance especially to bases and .. |
|||
Glass Transition Temp, Tg | -3.00 °C | 26.6 °F | |
Asahi Glass AFLAS® 100S TFE/P Fluoroelastomer AFLAS® 100/150 fluoroelastomers are alternating copolymers of tetrafluoroethylene and propylene. They offer 1) excellent heat resistance, 2) exceptional chemical resistance especially to bases and .. |
|||
Glass Transition Temp, Tg | -3.00 °C | 26.6 °F | |
Asahi Glass AFLAS® 150C TFE/P Fluoroelastomer AFLAS® 100/150 fluoroelastomers are alternating copolymers of tetrafluoroethylene and propylene. They offer 1) excellent heat resistance, 2) exceptional chemical resistance especially to bases and .. |
|||
Glass Transition Temp, Tg | -3.00 °C | 26.6 °F | |
Asahi Glass AFLAS® 150CS TFE/P Fluoroelastomer AFLAS® 100/150 fluoroelastomers are alternating copolymers of tetrafluoroethylene and propylene. They offer 1) excellent heat resistance, 2) exceptional chemical resistance especially to bases and .. |
|||
Glass Transition Temp, Tg | -3.00 °C | 26.6 °F | |
Asahi Glass AFLAS® 150E TFE/P Fluoroelastomer AFLAS® 100/150 fluoroelastomers are alternating copolymers of tetrafluoroethylene and propylene. They offer 1) excellent heat resistance, 2) exceptional chemical resistance especially to bases and .. |
|||
Glass Transition Temp, Tg | -3.00 °C | 26.6 °F | |
Asahi Glass AFLAS® 150P TFE/P Fluoroelastomer AFLAS® 100/150 fluoroelastomers are alternating copolymers of tetrafluoroethylene and propylene. They offer 1) excellent heat resistance, 2) exceptional chemical resistance especially to bases and .. |
|||
Glass Transition Temp, Tg | -3.00 °C | 26.6 °F | |
Asahi Glass AFLAS® SZ TFE/P/VdF Fluoroelastomer AFLAS® SZ/SP are terpolymers containing tetrafluoroethylene, propylene, and a small amount of vinylidene fluoride used as a cure site monomer. This combination gives AFLAS® SZ/SP a good balance of.. |
|||
Glass Transition Temp, Tg | -3.00 °C | 26.6 °F | |
Asahi Glass AFLAS® SP TFE/P/VdF Fluoroelastomer AFLAS® SZ/SP are terpolymers containing tetrafluoroethylene, propylene, and a small amount of vinylidene fluoride used as a cure site monomer. This combination gives AFLAS® SZ/SP a good balance of.. |