Thermal Properties Metric English Comments
Glass Transition Temp, Tg 28.8 °C
83.9 °F
ASTM D3417/D3418
SABIC Innovative Plastics Valox® FR1 Polybutylene Terephthalate Film, Flame Retardant
Valox FR-1 film is a flame retardant thermoplastic polybutylene, terephthalite film offering UL94 VTM-0 performance down to 125 microns and good temperature performance. Valox FR-1 film’s outst..