Thermal Properties | Metric | English | Comments |
---|---|---|---|
Glass Transition Temp, Tg | 31.0 °C | 87.8 °F | TM R050-25 |
Resinlab® EP1290 Clear Mineral Filled Epoxy Adhesive Resinlab™ EP1290 Clear is a two part mineral filled epoxy adhesive designed for bonding metals and plastics. It cures at room temperature to a tough, semi-flexible material. It has good wetting to .. |
|||
Glass Transition Temp, Tg | 31.0 °C | 87.8 °F | Ultimate Tg |
Tra-Con Tra-Coat 15D UV Curable Coating Adhesive The TRA-COAT 15D is a clear, liquid material that cures in thick sections to a "lens-like" appearance when exposed to ultra violet light. It`s rigidity makes it an ideal material for the coating of .. |
|||
Glass Transition Temp, Tg | 31.0 °C | 87.8 °F | TM R050-25 |
Resinlab® EP1290 Gray Mineral Filled Epoxy Adhesive Resinlab™ EP1290 Gray is a two part mineral filled epoxy adhesive designed for bonding metals and plastics. It cures at room temperature to a tough, semi-flexible material. It has good wetting to m.. |
|||
Glass Transition Temp, Tg | 31.0 °C | 87.8 °F | |
Loctite® 3887 High Adhesion Isotropic Epoxy Adhesive Electrically Conductive BondersLoctite® Electrically Conductive Adhesives are used in a variety of applications where electrical connectivity is needed, providing a conductive path where traditiona.. |
|||
Glass Transition Temp, Tg | 31.0 °C | 87.8 °F | DSC |
Lubrizol ESTANE® 5778 Ester Based Thermoplastic Polyurethane Features: It is especially well suited for dispersing co-ferrite as well as Cr02 pigments used in video, audio, and data storage applications. This product offers excellent hydrolytic stability unde.. |