Thermal Properties Metric English Comments
Glass Transition Temp, Tg >= 163 °C
>= 325 °F
ASTM D3418
BCC Products EB 6200 Epoxy Tooling Board
EB6200 is a “grain-free” elevated temperature epoxy modeling material known for its superior surface finish, dimensional stability and the ability to maintain tolerances even after being subjected..