Thermal Properties | Metric | English | Comments |
---|---|---|---|
Glass Transition Temp, Tg | 2.78 °C | 37.0 °F | ASTM D1329 |
Seals Eastern 7182D Fluorocarbon-Elastomer Formulated AFLAS® high-temperature "sour" oil & gas service. Excellent acid and base resistance.Information provided by Seals Eastern, Inc. |
|||
Glass Transition Temp, Tg | 2.78 °C | 37.0 °F | ASTM D1329 |
Seals Eastern 7182E Fluorocarbon-Elastomer Formulated AFLAS® high-temperature "sour" oil & gas service. Excellent acid and base resistance.Information provided by Seals Eastern, Inc. |
|||
Glass Transition Temp, Tg | 2.78 °C | 37.0 °F | ASTM D1329 |
Seals Eastern 7182X Fluorocarbon-Elastomer Formulated AFLAS®. Ultra-low compressive stress relaxation for alkaline, high-temperature service.Information provided by Seals Eastern, Inc. |
|||
Glass Transition Temp, Tg | 2.78 °C | 37.0 °F | ASTM D1329 |
Seals Eastern 7182A Fluorocarbon-Elastomer Formulated AFLAS® high-temperature, high-pressure "sour" oil & gas service. Resistant to extrusion. Excellent acid and base resistance.Information provided by Seals Eastern, Inc. |
|||
Glass Transition Temp, Tg | 2.78 °C | 37.0 °F | ASTM D1329 |
Seals Eastern 7182B Fluorocarbon-Elastomer Formulated AFLAS® high-temperature, high-pressure "sour" oil & gas service. ED resistant. Excellent acid and base resistance.Information provided by Seals Eastern, Inc. |