Thermal Properties | Metric | English | Comments |
---|---|---|---|
Glass Transition Temp, Tg | -51.1 - 3.00 °C | -60.0 - 37.4 °F | Average value: -18.6 °C Grade Count:174 |
Overview of materials for Thermoset Fluoroelastomer This property data is a summary of similar materials in the MatWeb database for the category "Thermoset Fluoroelastomer". Each property range of values reported is minimum and maximum values of appr.. |