Thermal Properties | Metric | English | Comments |
---|---|---|---|
Glass Transition Temp, Tg | 185 - 265 °C | 365 - 509 °F | Average value: 221 °C Grade Count:4 |
Overview of materials for Polysulfone, 20% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polysulfone, 20% Glass Fiber Reinforced". Specific grades with glass content between 15% and 24% are inc.. |
|||
Glass Transition Temp, Tg | 187 - 265 °C | 369 - 509 °F | Average value: 232 °C Grade Count:3 |
Overview of materials for Polysulfone, 30% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polysulfone, 30% Glass Fiber Reinforced". Specific grades with glass content between 25% and 34% are inc.. |