Polymer Property : Glass Transition Temp, Tg = 62.6 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Glass Transition Temp, Tg 17.0 °C
62.6 °F
Mallard Creek Polymers BarrierPro® 4545 SBR Emulsion
BARRIER PRO® 4545 is an anionic carboxylated styrene-butadiene copolymer latex. Features: highly stable, good compatibility with fillers and pigments, etc., cured films are tough and pliable, cur..
Glass Transition Temp, Tg 17.0 °C
62.6 °F
Mallard Creek Polymers ROVENE® 4041 SBR Latex
ROVENE® 4041 is a freeze-thaw stable carboxylated styrene-butadiene emulsion that can be used as a modifier for concrete applications. Concrete modified with ROVENE® 4041 is much tougher, more..
Glass Transition Temp, Tg 17.0 °C
62.6 °F
Mallard Creek Polymers TYKOTE® 1004 SBR Emulsion
TYKOTE® 1004 is an anionic carboxylated styrene-butadiene copolymer latex. Features: exceptional water resistance, exceptional grease resistance, pigment compatible, very high tensile strength, ..