Thermal Properties | Metric | English | Comments |
---|---|---|---|
Glass Transition Temp, Tg | 339 °C | 643 °F | Dry, Storage Modulus |
Renegade Materials Corporation MVK-14 Polyimide FreeForm™ IM7 12K Carbon Unitape MVK-14 polyimide prepregs are a more affordable and easier-to-process, non-carcinogenic alternative to PMR-15 and other older polyimide chemistries. MVK-14 offers a more durable alternative to high-.. |