Thermal Properties | Metric | English | Comments |
---|---|---|---|
Glass Transition Temp, Tg | 353 °C | 667 °F | DSC; ASTM E1356-03 |
NeXolve Novastrat® 400 Polyimide Colorless polyimide with high temperature stability.NeXolve Novastrat® 400 is a colorless polyimide with a higher temperature stability than NeXolve’s LaRC™CP1, exhibiting a glass transition temp.. |