Thermal Properties | Metric | English | Comments |
---|---|---|---|
Glass Transition Temp, Tg | 7.50 °C | 45.5 °F | Ultimate Tg |
Tra-Con Tra-Duct 926K01 Long Work Life Flexible Silver-Filled Epoxy Adhesive TRA-DUCT 926K01 is recommended for electronic bonding, coating and sealing applications that require high flexibility coupled with excellent electrical and mechanical properties. This two-part epoxy.. |