Thermal Properties Metric English Comments
Glass Transition Temp, Tg 422 °C
792 °F
DMA
Park Electrochemical Nelcote® V-303 Polyimide Prepreg, 7781 E-Glass Reinforced
Nelcote® V-303 is non-MDA condensation polyimide prepreg with a service temperature of 600°F.Key Features and Benefits:600°F maximum service temperatureGood electrical properties for RF applicati..